Fundamentals of Tribology in Metal Forming Available to Purchase
-
Published:2017
Abstract
This article describes friction force as a function of normal force in dry forming. It focuses on metal forming operations usually classified as cold working and hot working based on metallurgical considerations. The article discusses surface flattening and roughening of workpiece asperities in metal forming. It presents advanced tribology models and results for friction in isothermal forging operations in which the tooling is maintained at a temperature close to that of the workpiece. The article provides information on heat transfer models. It discusses the effect of wear in manufacturing processes. The article concludes with information on the main categories of tool and die materials used for a variety of manufacturing application.
Steven R. Schmid, Jack Jeswiet, Fundamentals of Tribology in Metal Forming, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 725–734, https://doi.org/10.31399/asm.hb.v18.a0006370
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.