Process Control Considerations in Heat Treating Available to Purchase
-
Published:1998
Abstract
Control of temperature and furnace atmospheres has become increasingly critical to successful heat treating. Temperature instrumentation and control systems used in heat treating include temperature sensors, controllers, final control elements, measurement instruments, and set-point programmers. This article describes these items and discusses the classifications and control of furnace atmospheres. The article also describes the surface carbon control devices available for the wide variety of furnace atmospheres and evaluation of carbon control. Finally, the article provides a set of guidelines for safety procedures that are common to all industrial heat treating furnace installations.
Process Control Considerations in Heat Treating, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1000–1007, https://doi.org/10.31399/asm.hb.mhde2.a0003199
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.