Hot-rolled steel bars and other hot rolled steel shapes are produced from ingots, blooms, or billets converted from ingots, or from strand cast blooms and billets, and comprise a variety of sizes and cross sections. This article provides a brief discussion on mechanical properties, quality descriptors and chemical compositions of hot-rolled steel bars, cold-finished steel bars, steel wire rod and steel wire. It contains tables that provide size tolerances for cold-finished carbon steel bar and cold-finished alloy steel bar.
Topics
Properties and performance,
Material failure analysis,
Fractography,
Cast iron,
Steel,
Stainless steel,
High-strength low-alloy steel,
Steel powder,
Superalloys,
Metallography,
Metal-matrix composites,
Aluminum,
Processing, treatment, and fabrication,
Bars,
Rods and wires,
Chemical composition,
Mechanical properties,
Product quality descriptors
You do not currently have access to this chapter.
Citation
Steel Bar, Rod, and Wire, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 232–241, https://doi.org/10.31399/asm.hb.mhde2.a0003095
Download citation file:
Related Book Content
Cold-Finished Steel Bars
Properties and Selection: Irons, Steels, and High-Performance Alloys
Steel Wire Rod
Properties and Selection: Irons, Steels, and High-Performance Alloys
Properties of Cast Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Steel Sheet, Strip, and Plate
Metals Handbook Desk Edition (2nd Edition)
Tin and Tin Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Carbon and Low-Alloy Steel Sheet and Strip
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hot-Rolled Steel Bars and Shapes
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hydrogen Embrittlement of Posttensioning Wires
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
Inspection of Steel Bar and Wire
Inspection of Metals Understanding the Basics
Principles of Alloying
Alloying Understanding the Basics