Heat Treating of Steel
-
Published:1998
Abstract
This article describes the heat treating (stress relieving, normalizing, annealing, quenching, tempering, martempering, austempering, and age hardening) of different types of steels, including ultrahigh-strength steels, maraging steels, and powder metallurgy steels. Tabulating the recommended temperatures for normalizing and austenitizing, it provides information on mechanism, cooling media, principal variables, process procedures, and applications of heat treating. In addition, the article gives a short note on the cold and cryogenic treatment of steel.
Heat Treating of Steel, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 970–982, https://doi.org/10.31399/asm.hb.mhde2.a0003196