Book Chapter
Compacted Graphite Iron
-
Published:1998
Page range:
320 - 322
Abstract
This article discusses the graphite morphology, chemical composition, mechanical and physical properties, and applications of compacted graphite (CG) irons. It compares the selected properties of gray, ductile and CG irons, and lists their property requirements as per ASTM A 842. A listing of tensile properties of various CG irons produced by different melt treatment methods is also provided.
You do not currently have access to this chapter.
Citation
Compacted Graphite Iron, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 320–322, https://doi.org/10.31399/asm.hb.mhde2.a0003109
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Specification, Selection, and Applications of Compacted Graphite Irons
Cast Iron Science and Technology
Compacted Graphite Iron Castings
Casting
Fatigue and Fracture Properties of Cast Irons
Fatigue and Fracture
Compacted Graphite Iron
Properties and Selection: Irons, Steels, and High-Performance Alloys
Wear of Cast Irons
Friction, Lubrication, and Wear Technology
Engineering Compacted Graphite Iron Castings
Iron and Steel Castings Engineering Guide
Engineering Ductile Iron Castings
Iron and Steel Castings Engineering Guide
Compacted Graphite Irons
Alloying Understanding the Basics
Mechanical Properties of Gray Irons
Cast Iron Science and Technology
Classification and Basic Types of Cast Iron
Cast Iron Science and Technology