Very High Density Metals
By
Kenneth H. Eckelmeyer
;
Kenneth H. Eckelmeyer
Sandia National Laboratories
Search for other works by this author on:
Steven G. Caldwell
Steven G. Caldwell
Teledyne Advanced Materials
Search for other works by this author on:
-
Published:1998
Abstract
Very high density materials are used for such applications as counterweights and radiation shields. This article focuses on the metallurgy, processing, properties, fabrication, design considerations, health and safety considerations, and applications of the most commonly used very high density materials: depleted uranium and tungsten and their alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Kenneth H. Eckelmeyer, Steven G. Caldwell, Very High Density Metals, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 691–695, https://doi.org/10.31399/asm.hb.mhde2.a0003166
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Uranium and Uranium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Heat Treating of Uranium and Uranium Alloys
Heat Treating of Nonferrous Alloys
Machining of Uranium and Uranium Alloys
Machining
Forging of Refractory Metals
Metalworking: Bulk Forming
Titanium Powder Metallurgy Products
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
P/M Stainless Steels
Metals Handbook Desk Edition (2nd Edition)
Annealing of Refractory Metals
Heat Treating of Nonferrous Alloys
Metallography and Microstructures of Uranium and Its Alloys
Metallography and Microstructures
Environmentally Assisted Cracking of Uranium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Glossary of Terms: Composites
Composites