Corrosion Resistance of Titanium and Titanium Alloys Available to Purchase
Editing author
-
Published:1998
Abstract
This article discusses corrosion resistance of titanium and titanium alloys to different types of corrosion, including galvanic corrosion, crevice corrosion, stress-corrosion cracking (SCC), erosion-corrosion, cavitation, hot salt corrosion, accelerated crack propagation, and solid and liquid metal embrittlement. A short section discusses the addition of alloys that can improve the corrosion resistance of titanium.
Rodney R. Boyer, Corrosion Resistance of Titanium and Titanium Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 584–585, https://doi.org/10.31399/asm.hb.mhde2.a0003142