Corrosion of Wrought Stainless Steels
-
Published:1998
Abstract
Selection of appropriate grades of steel will enable the steel to perform for very long times with minimal corrosion, but an inadequate grade can corrode and perforate more rapidly than a plain carbon steel will fail by uniform corrosion. This article describes the effect of chemical composition, heat treatment, welding, and surface condition on corrosion resistance of stainless steels. It discusses the various forms of corrosion and the important factors to be considered when selecting suitable stainless steel for application in specific corrosive environments.
Corrosion of Wrought Stainless Steels, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 379–386, https://doi.org/10.31399/asm.hb.mhde2.a0003117