A sliding bearing (plain bearing) is a machine element designed to transmit loads or reaction forces to a shaft that rotates relative to the bearing. This article explains the role of wear damage mechanisms in the design and selection of bearing materials, and its relationship with bearing material properties. Sliding bearings are commonly classified by terms that describe their application; they also are classified according to material construction, as single-metal, bimetal, or trimetal sliding bearings. The article further provides detailed tabular data on the designation and composition of the following types of bearing materials: tin-base alloys, lead-base alloys, copper-base...
Sign in
ASM members
Member Sign InMaterials for Sliding Bearings, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 695–701, https://doi.org/10.31399/asm.hb.mhde2.a0003167
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!