Abstract
Magnetic field testing includes some widely used nondestructive evaluation methods to inspect magnetic materials for defects such as cracks, voids, and inclusions and to assess other material properties, such as grain size, texture, and hardness. This article discusses the principles of such defect detection, providing details on the origin, generation, and assessment of leakage field data. In addition, it discusses the metallurgical and magnetic properties of magnetic materials and the applications of magnetic field testing.
Topics
Properties and performance,
Material failure analysis,
Fractography,
Cast iron,
Steel,
Stainless steel,
High-strength low-alloy steel,
Steel powder,
Superalloys,
Metallography,
Metal-matrix composites,
Aluminum,
Processing, treatment, and fabrication,
Manufacturing defects,
Nondestructive testing,
Magnetic leakage field testing
You do not currently have access to this chapter.
Citation
Magnetic Field Testing, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1273–1275, https://doi.org/10.31399/asm.hb.mhde2.a0003233
Download citation file:
Related Book Content
Techniques for Diagnosis of Corrosion Failures
Corrosion: Understanding the Basics
Microstructure and Domain Imaging of Magnetic Materials
Metallography and Microstructures