General Introduction to Surface Engineering
-
Published:1998
Page range:
1125 - 1126
Abstract
This article is a general introduction to surface engineering of engineering components, providing an overview of the applications of surface treatments and the environmental protection regulations directly or indirectly related to surface engineering processes.
You do not currently have access to this chapter.
Citation
General Introduction to Surface Engineering, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1125–1126, https://doi.org/10.31399/asm.hb.mhde2.a0003212
Download citation file:
Related Book Content
Engineering Component Configuration
Aluminum Castings Engineering Guide
Foreword
Introduction to Thin Film Deposition Techniques: Key Topics in Materials Science and Engineering
Preface
Introduction to Thin Film Deposition Techniques: Key Topics in Materials Science and Engineering
About the Author
Introduction to Thin Film Deposition Techniques: Key Topics in Materials Science and Engineering
Publication History
Surface Engineering
Foreword
Surface Engineering
Preface
Surface Engineering
Credits
Surface Engineering
Fatigue Fracture Appearances
Failure Analysis and Prevention (2021 Edition)
Surface Engineering of Nonferrous Metals
Metals Handbook Desk Edition (2nd Edition)