Abstract
This article describes the mechanism, advantages and disadvantages, fundamentals, capabilities, variations, equipment used, and weldability of metals in solid-state welding processes, including diffusion bonding, explosion welding, friction welding, ultrasonic welding, upset welding, and deformation welding.
You do not currently have access to this chapter.
Citation
Solid-State Welding Processes, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1104–1106, https://doi.org/10.31399/asm.hb.mhde2.a0003209
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Solid-State Welding and Bonding
Joining Understanding the Basics
Joining of Oxide-Dispersion-Strengthened Materials
Welding, Brazing, and Soldering
Safe Welding Practices
Welding Fundamentals and Processes
Modeling of Diffusion Bonding
Metals Process Simulation
Welding of Plastics
Welding, Brazing, and Soldering
Explosion Welding
Welding, Brazing, and Soldering
Procedure Development and Practice Considerations for Explosion Welding
Welding, Brazing, and Soldering
Resistance Welding
Joining Understanding the Basics
Fundamentals of Explosion Welding
Welding, Brazing, and Soldering
Upset Welding
Welding, Brazing, and Soldering