Metals Handbook Desk Edition (2nd Edition)
This volume is a comprehensive reference source on the properties, selection, processing, testing, and characterization of metals and their alloys. Compiled principally from the ASM Handbook series, coverage is organized into five major parts. The first part features a collection of engineering property data and guidance on the structure and properties of metallic materials. It also includes articles covering engineering design and materials selection. The second part provides detailed coverage of the properties and selection of ferrous alloys and heat-resistant superalloys. Information is presented on irons, carbon and alloy steels, stainless steels, and powder metallurgy steels. The third part covers nonferrous alloys and special-purpose materials such as metal-matrix composites and structural intermetallics. The fourth part addresses processing methods, including detailed information on casting, heat treating and joining. The final section covers testing, inspection, characterization, failure analysis, fractography, and metallography. The volume includes a comprehensive glossary of metallurgical and metalworking terms and definitions. For information on the print version of the Metals Handbook Desk Edition, 2nd Edition, ISBN 978-0-87170-654-6, follow this link
Download citation file:
Table of Contents
-
General Information
-
Structure and Properties of Metals
-
The Chemical ElementsByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on: -
Crystal Structure of Metallic ElementsByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on: -
Alloy Phase Diagrams and MicrostructureByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on: -
Properties of MetalsByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on:
-
-
Design Considerations and Materials Selection
-
Irons, Steels, and High-Performance Alloys
-
Structure/Property Relationships in Irons and SteelsByBruce L. BramfittBruce L. BramfittHomer Research Laboratories, Bethlehem Steel CorporationSearch for other works by this author on:
-
Steelmaking Practices and Their Influence on PropertiesByB. MishraB. MishraDepartment of Metallurgical & Materials Engineering, Colorado School of MinesSearch for other works by this author on:
-
-
Carbon and Alloy Steels
-
Cast Irons
-
Ferrous Powder Metallurgy Materials
-
Tool Steels
-
Stainless Steels
-
Superalloys
-
SuperalloysByMatthew J. Donachie;Matthew J. DonachieRensselaer at HartfordSearch for other works by this author on:Stephen J. DonachieStephen J. DonachieSpecial Metals CorporationSearch for other works by this author on:
-
-
Aluminum and Aluminum Alloys
-
Copper and Copper Alloys
-
Magnesium and Magnesium Alloys
-
Titanium and Titanium Alloys
-
Introduction and Overview of Titanium and Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on: -
Processing of Titanium and Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on: -
Corrosion Resistance of Titanium and Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on: -
Properties, Compositions, and Applications of Selected Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on:
-
-
Zinc and Zinc Alloys
-
Tin and Tin Alloys
-
Lead and Lead Alloys
-
Nickel and Nickel Alloys
-
Cobalt and Cobalt Alloys
-
Zirconium and Hafnium
-
Precious Metals and Alloys
-
Refractory Metals and Alloys
-
Cemented Carbides and Cermets
-
Special-Purpose Materials
-
Very High Density MetalsByKenneth H. Eckelmeyer;Kenneth H. EckelmeyerSandia National LaboratoriesSearch for other works by this author on:Steven G. CaldwellSteven G. CaldwellTeledyne Advanced MaterialsSearch for other works by this author on:
-
BiomaterialsByMatthew DonachieMatthew DonachieBiomedical Engineering Alliance for Connecticut (BEACON) and Rensselaer at HartfordSearch for other works by this author on:
-
Extractive Metallurgy
-
Extractive MetallurgyByB. MishraB. MishraDepartment of Metallurgical & Materials Engineering, Colorado School of MinesSearch for other works by this author on:
-
-
Casting
-
General Introduction to CastingByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
Solidification of Metals and AlloysByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
Molding MethodsByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
Melting MethodsByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
Foundry Practice for Ferrous AlloysByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
Foundry Practice for Nonferrous AlloysByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
Casting Design and Quality AssuranceByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:
-
-
Forming
-
Forging
-
Powder Metallurgy
-
Machining
-
Heat Treating
-
Joining
-
Surface Engineering
-
Recycling and Life-Cycle Analysis
-
RecyclingByJohn C. BittenceJohn C. BittenceWelshfield Studios
Editing author
Search for other works by this author on: -
Design for Recycling and Life-Cycle AnalysisByJohn C. BittenceJohn C. BittenceWelshfield Studios
Editing author
Search for other works by this author on:
-
-
Failure Analysis
-
Fractography
-
Nondestructive Testing
-
Mechanical, Wear, and Corrosion Testing
-
Wear TestingByPeter J. BlauPeter J. BlauMetals and Ceramics Division, Oak Ridge National LaboratorSearch for other works by this author on:
-
Metallography
-
Metallographic Practices Generally Applicable to All MetalsByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editor
Search for other works by this author on: -
Metallographic Technique for Ferrous MetalsByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on: -
Typical Microstructures of Iron-Base AlloysByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on: -
Metallographic Technique for Nonferrous Metals and Special-Purpose AlloysByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on: -
Measurement of MicrostructureByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on:
-
-
Materials Characterization
-
Introduction and Overview of Materials CharacterizationByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:
-
Bulk Elemental AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:
-
X-Ray Diffraction for Bulk Structural AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:
-
Microstructural AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:
-
Surface AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:
-
-
Reference Information