Metals Handbook Desk Edition (2nd Edition)Available to Purchase
This volume is a comprehensive reference source on the properties, selection, processing, testing, and characterization of metals and their alloys. Compiled principally from the ASM Handbook series, coverage is organized into five major parts. The first part features a collection of engineering property data and guidance on the structure and properties of metallic materials. It also includes articles covering engineering design and materials selection. The second part provides detailed coverage of the properties and selection of ferrous alloys and heat-resistant superalloys. Information is presented on irons, carbon and alloy steels, stainless steels, and powder metallurgy steels. The third part covers nonferrous alloys and special-purpose materials such as metal-matrix composites and structural intermetallics. The fourth part addresses processing methods, including detailed information on casting, heat treating and joining. The final section covers testing, inspection, characterization, failure analysis, fractography, and metallography. The volume includes a comprehensive glossary of metallurgical and metalworking terms and definitions. For information on the print version of the Metals Handbook Desk Edition, 2nd Edition, ISBN 978-0-87170-654-6, follow this link
Download citation file:
Table of Contents
-
General Information
-
Structure and Properties of Metals
-
The Chemical ElementsByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on:Published:01 December 1998 -
Crystal Structure of Metallic ElementsByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on:Published:01 December 1998 -
Alloy Phase Diagrams and MicrostructureByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on:Published:01 December 1998 -
Properties of MetalsByHugh BakerHugh BakerASM International
Consulting Editor
Search for other works by this author on:Published:01 December 1998
-
-
Design Considerations and Materials Selection
-
Irons, Steels, and High-Performance Alloys
-
Structure/Property Relationships in Irons and SteelsByBruce L. BramfittBruce L. BramfittHomer Research Laboratories, Bethlehem Steel CorporationSearch for other works by this author on:Published:01 December 1998
-
Steelmaking Practices and Their Influence on PropertiesByB. MishraB. MishraDepartment of Metallurgical & Materials Engineering, Colorado School of MinesSearch for other works by this author on:Published:01 December 1998
-
-
Carbon and Alloy Steels
-
Classifications and Designations of Carbon and Alloy SteelsPublished:01 December 1998
-
Mechanical Properties of Carbon and Alloy SteelsPublished:01 December 1998
-
High-Strength Structural and High-Strength Low-Alloy SteelsPublished:01 December 1998
-
Service Characteristics of Carbon and Alloy SteelsPublished:01 December 1998
-
Corrosion Characteristics of Carbon and Alloy SteelsPublished:01 December 1998
-
-
Cast Irons
-
Ferrous Powder Metallurgy Materials
-
Pressed-and-Sintered Ferrous Powder Metallurgy PartsPublished:01 December 1998
-
-
Tool Steels
-
Stainless Steels
-
Wrought Stainless Steels: Selection and ApplicationPublished:01 December 1998
-
-
Superalloys
-
SuperalloysByMatthew J. Donachie;Matthew J. DonachieRensselaer at HartfordSearch for other works by this author on:Stephen J. DonachieStephen J. DonachieSpecial Metals CorporationSearch for other works by this author on:Published:01 December 1998
-
-
Aluminum and Aluminum Alloys
-
Alloy and Temper Designation Systems for AluminumPublished:01 December 1998
-
Corrosion Resistance of Aluminum and Aluminum AlloysPublished:01 December 1998
-
Copper and Copper Alloys
-
Introduction and Overview of Copper and Copper AlloysPublished:01 December 1998
-
Thermal Softening and Stress Relaxation in CopperPublished:01 December 1998
-
Corrosion Characteristics of Copper and Copper AlloysPublished:01 December 1998
-
-
Magnesium and Magnesium Alloys
-
Selection and Applications of Magnesium and Magnesium AlloysPublished:01 December 1998
-
Corrosion Resistance of Magnesium and Magnesium AlloysPublished:01 December 1998
-
-
Titanium and Titanium Alloys
-
Introduction and Overview of Titanium and Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on:Published:01 December 1998 -
Processing of Titanium and Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on:Published:01 December 1998 -
Corrosion Resistance of Titanium and Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on:Published:01 December 1998 -
Properties, Compositions, and Applications of Selected Titanium AlloysByRodney R. BoyerRodney R. BoyerBoeing Commercial Airplane Company
Editing author
Search for other works by this author on:Published:01 December 1998
-
-
Zinc and Zinc Alloys
-
Tin and Tin Alloys
-
Lead and Lead Alloys
-
Nickel and Nickel Alloys
-
Cobalt and Cobalt Alloys
-
Zirconium and Hafnium
-
Precious Metals and Alloys
-
Refractory Metals and Alloys
-
Cemented Carbides and Cermets
-
Special-Purpose Materials
-
Very High Density MetalsByKenneth H. Eckelmeyer;Kenneth H. EckelmeyerSandia National LaboratoriesSearch for other works by this author on:Steven G. CaldwellSteven G. CaldwellTeledyne Advanced MaterialsSearch for other works by this author on:Published:01 December 1998
-
BiomaterialsByMatthew DonachieMatthew DonachieBiomedical Engineering Alliance for Connecticut (BEACON) and Rensselaer at HartfordSearch for other works by this author on:Published:01 December 1998
-
Extractive Metallurgy
-
Extractive MetallurgyByB. MishraB. MishraDepartment of Metallurgical & Materials Engineering, Colorado School of MinesSearch for other works by this author on:Published:01 December 1998
-
-
Casting
-
General Introduction to CastingByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
Solidification of Metals and AlloysByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
Molding MethodsByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
Melting MethodsByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
Foundry Practice for Ferrous AlloysByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
Foundry Practice for Nonferrous AlloysByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
Casting Design and Quality AssuranceByThomas S. PiwonkaThomas S. PiwonkaThe University of AlabamaSearch for other works by this author on:Published:01 December 1998
-
-
Forming
-
Forming of Stainless Steel and Heat-Resistant AlloysPublished:01 December 1998
-
Forging
-
Powder Metallurgy
-
Machining
-
Surface Finish and Surface Integrity in MachiningPublished:01 December 1998
-
Heat Treating
-
Basic Principles and Design Guidelines for Heat Treating of SteelPublished:01 December 1998
-
Process Control Considerations in Heat TreatingPublished:01 December 1998
-
Heat Treating of Stainless Steels and Heat-Resistant AlloysPublished:01 December 1998
-
-
Joining
-
Surface Engineering
-
Chemical Vapor Deposition and Related ProcessesPublished:01 December 1998
-
Surface Engineering of Stainless Steels and Heat-Resistant AlloysPublished:01 December 1998
-
Recycling and Life-Cycle Analysis
-
RecyclingByJohn C. BittenceJohn C. BittenceWelshfield Studios
Editing author
Search for other works by this author on:Published:01 December 1998 -
Design for Recycling and Life-Cycle AnalysisByJohn C. BittenceJohn C. BittenceWelshfield Studios
Editing author
Search for other works by this author on:Published:01 December 1998
-
-
Failure Analysis
-
Engineering Aspects of Failure and Failure AnalysisPublished:01 December 1998
-
Failures from Various Mechanisms and Related Environmental FactorsPublished:01 December 1998
-
-
Fractography
-
Nondestructive Testing
-
Guide to Nondestructive Testing and Inspection MethodsPublished:01 December 1998
-
-
Mechanical, Wear, and Corrosion Testing
-
Wear TestingByPeter J. BlauPeter J. BlauMetals and Ceramics Division, Oak Ridge National LaboratorSearch for other works by this author on:Published:01 December 1998
-
Metallography
-
Metallographic Practices Generally Applicable to All MetalsByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editor
Search for other works by this author on:Published:01 December 1998 -
Metallographic Technique for Ferrous MetalsByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on:Published:01 December 1998 -
Typical Microstructures of Iron-Base AlloysByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on:Published:01 December 1998 -
Metallographic Technique for Nonferrous Metals and Special-Purpose AlloysByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on:Published:01 December 1998 -
Measurement of MicrostructureByGeorge F. Vander VoortGeorge F. Vander VoortBuehler Ltd.
Editing author
Search for other works by this author on:Published:01 December 1998
-
-
Materials Characterization
-
Introduction and Overview of Materials CharacterizationByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:Published:01 December 1998
-
Bulk Elemental AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:Published:01 December 1998
-
X-Ray Diffraction for Bulk Structural AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:Published:01 December 1998
-
Microstructural AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:Published:01 December 1998
-
Surface AnalysisByK.H. EckelmeyerK.H. EckelmeyerMicrostructural Analysis Department, Sandia National LaboratoriesSearch for other works by this author on:Published:01 December 1998
-
-
Reference Information
-
Glossary of Metallurgical and Metalworking TermsPublished:01 December 1998
-