Electrical/Electronic Applications for Advanced Ceramics
-
Published:1995
Abstract
Ceramic materials serve important insulative, capacitive, conductive, resistive, sensor, electrooptic, and magnetic functions in a wide variety of electrical and electronic circuitry. This article focuses on various applications of advanced ceramics in both electric power and electronics industry, namely, dielectric, piezoelectric, ferroelectric, sensing, magnetic and superconducting devices.
Electrical/Electronic Applications for Advanced Ceramics, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 1016–1056, https://doi.org/10.31399/asm.hb.emde.a0003062