General Additives for Plastics and Elastomers
-
Published:1995
Abstract
Additives for plastics and elastomers are used to increase the ease of processing and to improve the properties of the final product. Additives improve processing characteristics by increasing lubricity and by stabilizing the polymer. Additives that improve properties include those that decrease static charge development and microbial activity and those that improve flame retardation characteristics, color, light stability, impact resistance, density and mechanical properties. This article focuses on the additives for polymers and elastomers that are used for improving processing--blowing agents, mold-release agents, lubricants, plasticizers, and heat stabilizers--and for improving properties antimicrobials, antioxidants, antistatic agents, colorants, fillers and fiber reinforcements, flame retardants, impact modifiers, light stabilizers, plasticizers, and heat stabilizers. Furthermore, it discusses the method for addition of these additives and the problems faced during compounding.
General Additives for Plastics and Elastomers, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 287–291, https://doi.org/10.31399/asm.hb.emde.a0003012
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!