Thermoforming
-
Published:1995
Abstract
Thermoforming is a manufacturing process in which thermoplastic sheets are heated, softened, clamped onto a mold, and made to conform to the shape of the mold or forming tool. It is ideally suited to large-volume runs of small items. This article focuses on major phases of thermoforming, namely, sheet transportation, heating, forming/cooling, and trimming, and different thermoforming techniques: basic female forming; basic male forming; matched-mold thermoforming; plug-assist thermoforming; pressure bubble plug-assist vacuum thermoforming; vacuum snapback thermoforming; air-slip thermoforming; and trapped-sheet, contact heat, and pressure thermoforming. It concludes with a discussion on machines and the economic concerns of thermoforming.
Thermoforming, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 327–331, https://doi.org/10.31399/asm.hb.emde.a0003018
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!