Engineering Thermoplastics
-
Published:1995
Page range:
180 - 205
Abstract
This article discusses the family characteristics, commercial forms, applications, resin grades, and mechanical and physical properties of traditional engineering thermoplastics in their neat (unmodified) form and as compounds and composites, namely, acrylonitrile-butadiene-styrenes, acrylics, high-density polyethylenes, reinforced polypropylenes, high-impact polystyrenes, polyvinyl chloride, styrene-acrylonitriles, and styrene-maleic anhydrides.
You do not currently have access to this chapter.
Citation
Engineering Thermoplastics, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 180–205, https://doi.org/10.31399/asm.hb.emde.a0003008
Download citation file:
Related Book Content
Blow Molding
Engineered Materials Handbook Desk Edition
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Explosion Welding
Welding, Brazing, and Soldering
Heat Treatment of Gears
Heat Treatment of Gears A Practical Guide for Engineers
Commercial Alloy Phase Diagrams and Their Industrial Applications
Metals Process Simulation
Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Corrosion of Nickel and Nickel-Base Alloys
Corrosion: Materials
Bulk Molding Compounds
Engineered Materials Handbook Desk Edition
Introduction to Aluminum and Aluminum Alloys
Metals Handbook Desk Edition (2nd Edition)
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys