Book Chapter
Joining of Ceramics
-
Published:1995
Page range:
846 - 864
Abstract
Many applications of ceramics and glasses require them to be joined to each other or to other materials such as metals. This article focuses on ceramic joining technologies, including glass-metal sealing, glass-ceramic/metal joining, ceramic-metal joining, ceramic-ceramic joining, and the more advanced joining of nonoxide ceramics. It also discusses metallizing, brazing, diffusion bonding, and chemical bonding.
You do not currently have access to this chapter.
Citation
Joining of Ceramics, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 846–864, https://doi.org/10.31399/asm.hb.emde.a0003056
Download citation file:
Related Book Content
Structural Ceramics
Lightweight Materials Understanding the Basics
Fundamentals of Diffusion Bonding
Welding, Brazing, and Soldering
Introduction
Principles of Soldering
Modeling of Diffusion Bonding
Metals Process Simulation
Chemistry Basics
Elementary Materials Science
Elemental Chemistry Introduction
Protective Organic Coatings
Metallizing of Plastics
Engineered Materials Handbook Desk Edition
History of Brazing
Principles of Brazing
Abbreviations and Symbols
Principles of Brazing
Selected References
Principles of Brazing