Engineering Tables: Ceramics and Glasses
-
Published:1995
Abstract
This article is a comprehensive collection of engineering property data in tabulated form for ceramics and glasses. Data are provided for physical and mechanical properties of ceramic materials and color of ceramics fired under oxidizing and reducing conditions. The article also lists the materials characterization techniques for ceramics and glasses.
Engineering Tables: Ceramics and Glasses, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 103–105, https://doi.org/10.31399/asm.hb.emde.a0003004