Abstract
This article is a comprehensive collection of engineering property data in tabulated form for ceramics and glasses. Data are provided for physical and mechanical properties of ceramic materials and color of ceramics fired under oxidizing and reducing conditions. The article also lists the materials characterization techniques for ceramics and glasses.
You do not currently have access to this chapter.
Citation
Engineering Tables: Ceramics and Glasses, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 103–105, https://doi.org/10.31399/asm.hb.emde.a0003004
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Characterization of Ceramics and Glasses
Materials Characterization (2019 Edition)
Introduction to Materials Characterization
Materials Characterization
Mechanical Behavior of Nonmetallic Materials
Mechanics and Mechanisms of Fracture An Introduction
Fatigue Testing of Brittle Solids
Mechanical Testing and Evaluation
Ceramic Materials
Materials for Medical Devices
Acoustic Microscopy
Nondestructive Evaluation of Materials
Glossary of Terms: Materials Characterization
Materials Characterization
Introduction to the Mechanical Behavior of Nonmetallic Materials
Mechanical Testing and Evaluation
Design and Engineering Properties of Glasses
Engineered Materials Handbook Desk Edition
Temper Colors for Steels
Heat Treating of Irons and Steels