This article is a compilation of tables containing property data for major reinforcement materials, including high-modulus fibers, carbon fibers, graphite fibers, glass fibers, ceramic short fibers and whiskers. Data are provided for physical, mechanical, chemical, thermal and electrical properties of these materials. Maximum service temperatures of whisker reinforcements also are provided.