Properties and Characteristics of Engineering Plastics and Elastomers
-
Published:1995
Abstract
Engineering plastics offer unique product benefits based on physical properties, or combinations of physical properties, that allow vastly improved product performance. Providing an overview of the general characteristics and the mechanical and environmental stress response of engineering plastics, this article discusses various factors, including thermal, mechanical and electrical properties, environmental factors, and material cost that are important in the selection of engineering plastics for specific applications.
Abstract
This article discusses the family characteristics, commercial forms, applications, resin grades, and mechanical and physical properties of traditional engineering thermoplastics in their neat (unmodified) form and as compounds and composites, namely, acrylonitrile-butadiene-styrenes,...
Sign in
ASM members
Member Sign InProperties and Characteristics of Engineering Plastics and Elastomers, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.