Testing of Adhesive Joints Available to Purchase
-
Published:2000
Abstract
Adhesive joints involve joining parts by bonding component parts together with an adhesive. This article provides a discussion on the purpose of testing adhesive joints and on the factors influencing mechanical strength of these joints. It describes the various tests used in the measurement of adhesive joint strength. These include qualitative tests, peel tests, lap shear tests, tensile tests, and adhesive fracture mechanics tests.
K.L. DeVries, Paul Borgmeier, Testing of Adhesive Joints, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 836–844, https://doi.org/10.31399/asm.hb.v08.a0003324