Property Comparison Tables: Hardness and Tensile Properties
-
Published:2000
Abstract
This article is a comprehensive collection of tables that list the values for hardness of plastics, rubber, elastomers, and metals. The tables also list the tensile yield strength and tensile modulus of metals and plastics at room temperature. A comparison of various engineering materials, on the basis of tensile strength, is also provided.
You do not currently have access to this chapter.
Citation
Property Comparison Tables: Hardness and Tensile Properties, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 935–938, https://doi.org/10.31399/asm.hb.v08.a0003331
Download citation file:
Related Book Content
Tribology of Plastics and Elastomers
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Mechanical Testing and Properties of Plastics—An Introduction
Characterization and Failure Analysis of Plastics
Hardness Measurement of Plastics and Elastomers
Hardness Testing Principles and Applications
Mechanical Testing and Properties of Plastics: An Introduction
Characterization and Failure Analysis of Plastics
Electrical Testing of Polymers
Engineered Materials Handbook Desk Edition
Introduction to Environmental Performance of Nonmetallic Materials
Corrosion: Materials
Tensile Testing of Elastomers
Tensile Testing (Second Edition)
Wear Failures of Plastics
Failure Analysis and Prevention
Environmental Performance of Elastomers
Corrosion: Materials
Plastic Design Methods
Characterization and Failure Analysis of Plastics