Mechanical Testing and Evaluation
Overview of Mechanical Properties and Testing for Design
-
Published:2000
Abstract
An integral aspect of designing and material selection is the use of mechanical properties derived from various mechanical testing. This article introduces the basic concepts of mechanical design and its relation with the properties derived from various mechanical testings, namely, tensile, compressive, hardness, torsion and bend, shear load, shock, and fatigue and creep testings. It describes the design criteria for combined properties derived from each of the mechanical testing. The article concludes with a discussion on the effect of environment on the mechanical properties.
Sign in
ASM members
Member Sign InHoward A. Kuhn, Overview of Mechanical Properties and Testing for Design, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 49–69, https://doi.org/10.31399/asm.hb.v08.a0003257
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!