Torsional Kolsky Bar Testing Available to Purchase
-
Published:2000
Abstract
This article provides a discussion on the generation of an incident wave with the help of the stored-torque torsional Kolsky bar and explosively loaded torsional Kolsky bar. It examines the procedures followed for measuring the waves in these bars. The article compares the compression Kolsky bar with the torsional Kolsky bar. It includes information on the various application areas of torsional Kolsky bar: limitations on strain rate, low- and high-temperature testing, quasi-static and incremental strain-rate testing, and localization and shear-banding experiments.
Amos Gilat, Torsional Kolsky Bar Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 505–515, https://doi.org/10.31399/asm.hb.v08.a0003300
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.