This article presents typical problems encountered in the analysis of experimental creep and creep-rupture data and the possible solutions to these drawbacks. It provides information on planning the test and creep strain/time relationships. The exponential creep equation and the rational polynomial creep equation are discussed. The article also describes the dependence of stress and temperature on equation parameters and explains the lot-centered regression analysis.