Fatigue Crack Growth Data Analysis[1]
-
Published:2000
Abstract
Fatigue crack growth rate testing and data analysis are performed to characterize the crack propagation resistance of material environment combinations in order to predict crack growth life under anticipated stress histories. This article presents analyses performed on the numerical output of crack growth rate tests, including the analysis framework for modeling fatigue crack growth rate data. It describes the numerical methods for calculating da/dN as a function of stress intensity factor. The article discusses the principles in fatigue crack growth damage analysis.
Sign in
ASM members
Member Sign InAlan P. Berens, Fatigue Crack Growth Data Analysis, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, https://doi.org/10.31399/asm.hb.v08.a0009217
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.