Triaxial Hopkinson Techniques
-
Published:2000
Abstract
Triaxial Hopkinson techniques can be used to simultaneously subject a sample to axial and lateral compressions. The lateral compression may be applied through a pneumatic pressure vessel or dynamically using a special Hopkinson technique. This article reviews these two techniques in detail. It illustrates a 75-mm Hopkinson system, particularly designed to test large samples of concrete, rock, polymeric composites, and other materials with relatively coarse microstructures. The article also provides information on the pneumatic pressure vessel for a 75-mm Hopkinson bar test system and the dynamic triaxial load cell on a 19-mm Hopkinson bar.
Sia Nemat-Nasser, Jon Isaacs, Jacob Rome, Triaxial Hopkinson Techniques, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 516–518, https://doi.org/10.31399/asm.hb.v08.a0003301
Download citation file:
Data Ecosystem
The ASM Data Ecosystem arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.