Miscellaneous hardness tests encompass a number of test methods that have been developed for specific applications. These include dynamic, or "rebound," hardness tests using a Leeb tester or a Scleroscope; static indentation tests on rubber or plastic products using the durometer or IRHD testers; scratch hardness tests; and ultrasonic microindentation testing. This article reviews the procedures, equipment, and applications associated with these alternate hardness test methods.