This article provides an overview of the safety aspects and integrity concept for pressure vessels, piping, and tubing. It focuses on the fracture mechanics approaches used to validate components with longitudinal cracks and circumferential cracks and to analyze crack growth behavior under cyclic loading. Full-scale testing facilities and the typical test results required for various applications are discussed. The article also presents information on the transferability of mechanical properties of materials.