Influence of Multiaxial Stresses on Creep and Creep Rupture of Tubular Components Available to Purchase
-
Published:2000
Abstract
This article presents effective stress equations that are based on the von Mises criterion, the Tresca criterion, and the Huddleston criterion. It describes the calculation of effective stresses for different cases: elastic stresses, steady-state creep stresses, stresses in a fully plastic case, and thermal stresses in a tube. The article illustrates the comparison of life predictions by the stress criteria and presents a simple mean diameter hoop stress equation, which is used for designing components. It also provides information on the multiaxial creep ductility of tubular components and multiaxial testing methods.
R.C. Hurst, J.H. Rantala, Influence of Multiaxial Stresses on Creep and Creep Rupture of Tubular Components, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 405–411, https://doi.org/10.31399/asm.hb.v08.a0003291
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.