Book Chapter
Macroindentation Hardness Testing
By
Edward L. Tobolski
Wilson Instruments Division, Instron Corporation
;
Edward L. Tobolski
Search for other works by this author on:
-
Published:2000
Abstract
This article describes the principal methods for macroindentation hardness testing by the Brinell, Vickers, and Rockwell methods. For each method, the test types and indenters, scale limitations, testing machines, calibration, indenter selection and geometry, load selection and impression size, testing methodology, and testing of specific materials are also discussed.
Topics
Creep testing,
Fatigue testing,
Impact toughness testing,
Hardness testing,
High strain rate shear testing,
Residual stress analysis,
Tensile testing,
Wear testing,
Macroindentation testing,
Brinell hardness testing,
Vickers hardness testing,
Rockwell hardness,
Measuring and testing instruments
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Edward L. Tobolski, Andrew Fee, Macroindentation Hardness Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 203–220, https://doi.org/10.31399/asm.hb.v08.a0003271
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Hardness Testing
Inspection of Metals Understanding the Basics
Standardization
Hardness Testing Principles and Applications
Hardness Measurement of Metals—Static Methods
Hardness Testing Principles and Applications
Introduction to Hardness Testing
Mechanical Testing and Evaluation
Instrumented Indentation Testing
Mechanical Testing and Evaluation
Particle-Induced X-Ray Emission
Materials Characterization
Potentiometric Membrane Electrodes
Materials Characterization
Gas Analysis by Mass Spectrometry
Materials Characterization
Accreditation of Mechanical Testing Laboratories
Mechanical Testing and Evaluation
Ultrasonic Imaging and Sizing
Nondestructive Evaluation of Materials