Mechanical Testing and Evaluation
High Strain Rate Tension and Compression Tests
-
Published:2000
Abstract
This article reviews high strain rate compression and tension test methods with a focus on the general principles, advantages, and limitations of each test method. The compression test methods are cam plastometer test, drop tower compression test, the Hopkinson bar in compression, and rod impact (Taylor) test. The flyer plate impact test, expanding ring test, split-Hopkinson bar in tension, and a test using a rotating wheel used for high strain rate tension are also discussed.
Sign in
ASM members
Member Sign InHigh Strain Rate Tension and Compression Tests, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 429–446, https://doi.org/10.31399/asm.hb.v08.a0003294