Testing of Bearings Available to Purchase
Retired
-
Published:2000
Abstract
This article provides an overview of two major classes of bearings: rolling bearings and sliding, or plain, bearings. It reviews the experimental data resulted from testing of rolling and sliding bearing materials with illustration. The article presents a table that summarizes rolling contact fatigue test methods that ASTM published in STP 771. It also describes the role of lubrication in the bearings.
Charles A. Moyer, Testing of Bearings, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 853–860, https://doi.org/10.31399/asm.hb.v08.a0003326