Book Chapter
Introduction to Creep and Stress-Relaxation Testing
By
James C. Earthman
University of California at Irvine
James C. Earthman
Search for other works by this author on:
-
Published:2000
Abstract
This article provides the theoretical background for understanding many of the physical processes relevant to mechanical testing methods, experimental results, and analytical approaches described in this volume.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
James C. Earthman, Introduction to Creep and Stress-Relaxation Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 361–362, https://doi.org/10.31399/asm.hb.v08.a0003286
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Creep Deformation of Metals, Polymers, Ceramics, and Composites
Mechanical Testing and Evaluation
Elevated-Temperature Life Assessment
Analysis and Prevention of Component and Equipment Failures
Creep and Creep-Rupture Testing
Mechanical Testing and Evaluation
High-Temperature Failures
Fatigue and Fracture Understanding the Basics
Mean Stress
Fatigue and Durability of Structural Materials
Creep
Damage Mechanisms and Life Assessment of High-Temperature Components
Annealing and Recrystallization of Coppers
Heat Treating of Nonferrous Alloys
Creep, Stress Relaxation, and Yielding
Characterization and Failure Analysis of Plastics
Creep and Stress Rupture Failures
Failure Analysis and Prevention
Mechanical Properties and Strengthening Mechanisms
Metallurgy for the Non-Metallurgist (Second Edition)