Mechanical Testing and Evaluation
Reference Information
-
Published:2000
Abstract
This article is a comprehensive collection of tables that list the values for hardness of plastics, rubber, elastomers, and metals. The tables also list the tensile yield strength and tensile modulus of metals and plastics at room temperature. A comparison of various engineering materials, on the basis of tensile strength, is also provided.
Abstract
This article is a compilation of terms related to mechanical testing and evaluation of metals, plastics, ceramics, and composites.
Sign in
ASM members
Member Sign InReference Information, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000