Component Testing
-
Published:2000
Abstract
This article describes the tests for the common types of fabricated components and modeling of metal deformation. It provides an overview of component testing and briefly reviews the relationship of mechanical properties in the process of mechanical design for static loads, cyclic loads, dynamic loads, and high-temperature materials. The article describes the general properties related to monotonic stress-strain behavior of steels. It also discusses materials properties and operating stresses as well as other factors, such as part shape and environmental effects, which play significant roles in the design process of components.
Abstract
Forming processes can be divided into three...
Sign in
ASM members
Member Sign InComponent Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.