Fatigue Testing
-
Published:2000
Abstract
The separation of the fatigue process into crack initiation and propagation phases has been an important and useful advance in engineering. The combined approach of strain-control testing and the development fracture mechanics of fatigue crack growth rates is a key advance that allows better understanding and simulation of both crack nucleation and the subsequent crack growth mechanisms. This article reviews three basic types of fatigue properties: stress-life, strain life, and fracture mechanic crack growth.
Abstract
This article describes the phenomena of crack initiation and early growth. It examines specimen design and preparation as well as the apparatus used in...
Sign in
ASM members
Member Sign InFatigue Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.