Corrosion Resistance of Stainless Steels and Nickel Alloys Available to Purchase
-
Published:2003
Abstract
Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This article examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on corrosion resistance of these materials. It provides information on the compositions of selected stainless steels, copper-nickel, and nickel-base alloys in a tabular form. The article also illustrates the compositional and property linkages for stainless steels and nickel-base alloys.
A. John Sedriks, Corrosion Resistance of Stainless Steels and Nickel Alloys, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 697–702, https://doi.org/10.31399/asm.hb.v13a.a0003676
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.