Corrosion Resistance of Magnesium Alloys
Revising author
-
Published:2003
Abstract
This article begins with a discussion on the corrosion characteristics of unalloyed magnesium and two major magnesium alloy systems. It shows the effects of iron and 13 other elements on the saltwater corrosion performance of magnesium in binary alloys with increasing levels of the individual elements. The article illustrates the effect of increasing iron, nickel, and copper contamination on the standard ASTM B 117 salt-spray performance of the die-cast AZ91 test specimens as compared to the range of performance observed for cold-rolled steel and die-cast aluminum alloy 380 samples. It discusses the effect of heat treating and cold working...
Sign in
ASM members
Member Sign InBarbara A. Shaw, Corrosion Resistance of Magnesium Alloys, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 692–696, https://doi.org/10.31399/asm.hb.v13a.a0003675
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.