Abstract
This article discusses factors that influence the effect of alloying, metallurgical treatments, and mechanical treatments on the corrosion resistance of metallic materials, with schematic illustrations.
You do not currently have access to this chapter.
Citation
Paul Natishan, Introduction to Corrosion Resistance of Bulk Materials, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 687–688, https://doi.org/10.31399/asm.hb.v13a.a0003673
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Introduction to Corrosion Resistance of Bulk Materials
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion
Titanium Physical Metallurgy, Processing, and Applications
Stainless Steels
Steels: Processing, Structure, and Performance (Second Edition)
Tensile Testing
Inspection of Metals Understanding the Basics
Principles of Alloying
Alloying Understanding the Basics
Periodic System for Ferrous Metallurgists
Fundamentals of Modeling for Metals Processing
Low-Expansion Alloys
Alloying Understanding the Basics
Magnetic Alloys
Alloying Understanding the Basics
Creep and Stress-Rupture Failures
Failure Analysis and Prevention (2021 Edition)
Fatigue Fracture of Waspaloy Spray-Manifold Assembly Because of Embrittlement by Penetration of Molten Braze Metal
ASM Failure Analysis Case Histories: Processing Errors and Defects