Statistical Interpretation of Corrosion Test Results
-
Published:2003
Abstract
This article details factors that have been used for evaluating the susceptibility of alloys to stress-corrosion cracking. Many considerations impacting the validity and accuracy of information gathered from laboratory testing programs are reviewed. The article highlights the main characteristics of probability distributions, such as normal distribution, log-normal distribution, exponential distribution, Poisson distribution, and extreme-value distribution. It also provides information on the statistical concepts to produce effective test programs.
Sign in
ASM members
Member Sign InP.R. Roberge, Statistical Interpretation of Corrosion Test Results, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 425–429, https://doi.org/10.31399/asm.hb.v13a.a0003641
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.