Pack Cementation Coatings
-
Published:2003
Abstract
This article focuses on the pack-cementation coatings, in particular, halide-activated pack cementation coatings on nickel alloys. It also describes the thermodynamics and kinetics of, and simultaneous deposition of various types of, pack cementation processes. These include pack aluminizing, chromizing, and siliconizing.
Vilupanur A. Ravi, Pack Cementation Coatings, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 763–771, https://doi.org/10.31399/asm.hb.v13a.a0003686