Anodes for Batteries
-
Published:2003
Abstract
This article examines constructive corrosion that occurs in power-generating devices, specifically batteries. It discusses the kinetic aspects of constructive corrosion in batteries and provides examples to illustrate how the kinetics of a corrosion process varies among different battery systems. The article illustrates the constructive roles played by corrosion at anodes in batteries through the use of a zinc anode in a mercury battery and a lithium metal anode in a rechargeable lithium battery. It also outlines the destructive role played by corrosion by illustrating shelf reactions in zinc-carbon batteries and lead grid corrosion in lead-acid batteries.
Sign in
ASM members
Member Sign InCharles F. Windisch, Jr., Anodes for Batteries, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 170–177, https://doi.org/10.31399/asm.hb.v13a.a0003601
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.