This article examines constructive corrosion that occurs in power-generating devices, specifically batteries. It discusses the kinetic aspects of constructive corrosion in batteries and provides examples to illustrate how the kinetics of a corrosion process varies among different battery systems. The article illustrates the constructive roles played by corrosion at anodes in batteries through the use of a zinc anode in a mercury battery and a lithium metal anode in a rechargeable lithium battery. It also outlines the destructive role played by corrosion by illustrating shelf reactions in zinc-carbon batteries and lead grid corrosion in lead-acid batteries.