Cathodic Protection
-
Published:2003
Abstract
Cathodic protection is an electrochemical means of corrosion control in which the oxidation reaction in a galvanic cell is concentrated at the anode, which suppresses corrosion of the cathode in the same cell. This article provides a detailed discussion on the fundamentals and types of cathodic protection as well as their power sources and design considerations. The criteria for the cathodic protection and types of materials used in sacrificial anodes and impressed-current anodes are also discussed. The article provides examples selected for familiarizing the design engineer with the steps for selecting a specific corrosion control method.
Robert H. Heidersbach, Cathodic Protection, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 855–870, https://doi.org/10.31399/asm.hb.v13a.a0003697
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.