Abstract
Vapor-deposition processes fall into two major categories, namely, physical vapor deposition (PVD) and chemical vapor deposition (CVD). This article describes major deposition processes such as sputtering, evaporation, ion plating, and CVD. The list of materials that can be vapor deposited is extensive and covers almost any coating requirement. The article provides a table of some corrosion-resistant vapor deposited materials. It concludes with an overview of the applications of CVD and PVD coatings and a discussion on coatings for graphite, the aluminum coating of steel, and alloy coatings for aircraft turbines, marine turbines, and industrial turbines.
Sign in
ASM members
Member Sign InCVD and PVD Coatings, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 759–762, https://doi.org/10.31399/asm.hb.v13a.a0003685
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.