Evaluating Uniform Corrosion
Revising author
-
Published:2003
Abstract
Uniform corrosion refers to the attack on an exposed metal surface that results in homogeneous thickness loss that is evaluated by mass loss or measurement of thickness change. This article focuses on the various processes involved in mass loss tests, namely, selection and preparation of suitable test specimens, planning of the experimental technique, posttest sample cleaning, data acquisition, and reporting. It further discusses the test variables addressed during the experimental planning and provides an overview of the other test and evaluation methods of evaluating uniform corrosion.
Sign in
ASM members
Member Sign InBopinder Phull, Evaluating Uniform Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 542–544, https://doi.org/10.31399/asm.hb.v13a.a0003660
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.